Sign In | Join Free | My hardware-wholesale.com |
|
Categories | Precision Alloy |
---|---|
Brand Name: | Tankii |
Model Number: | 1J79 |
Certification: | ISO 9001 |
Place of Origin: | CHINA |
MOQ: | 50 kg |
Price: | 30-35usd / kg |
Payment Terms: | T/T, Western Union |
Supply Ability: | 20000kg/month |
Delivery Time: | 5-30 days |
Packaging Details: | wooden case |
Shape: | ribbon |
Surface: | Bright |
Color: | gray |
Content: | FeNi |
Condition: | soft or hard |
Company Info. |
Shanghai Tankii Alloy Material Co.,Ltd |
Verified Supplier |
View Contact Details |
Product List |
1j79 Permalloy Strip E11c Strip Soft Magnetic Alloy ribbon for Magnetically Shielded
Classification: precision soft magnetic alloy
Supplement: Alloy with high permeability in weak fields at saturation
induction 0.65-0.75 T. Alloy 1J79/ permally high squareness of the
hysteresis loop and a low coefficient of magnetization reversal
Application: For small cores of transformers, chokes and relays operating in
weak fields, magnetic shields. In the small thickness (0.05 ± 0.02
mm) - cores for pulse transformers, magnetic amplifiers and solid
state relays
Chemical Composition,%:
Ni 78.5 - 80% | Fe 13.73 - 16.8% | C 0.03% | Si 0.3 - 0.5% | Mn 0.6 - 1.1% | S o 0.02% |
P 0.02% | Mo 3.8 - 4.1% | Ti 0.15% | Al 0.15% | Cu 0.2% |
Basic physical constants and mechanical properties of the alloy:
Density: γ = 8,6 g / cm3;
Electric resistivity: ρ = 0,55 ohm mm2 ? / m;
The temperature of the Curie point: Θs = 430 ° C;
Saturation magnetostriction: λS = 2 ? 106;
Brinell hardness of 210/120 HB;
Ultimate: RM = 1030/490 MPa;
Yield strength: σ0,2 = 980 145 MPa;
Modulus of elasticity E = 210 kN / mm2;
Elongation: δ5 = 3/50%;
Relative compression: φ = -%.
Heat treatment of the alloy
Annealing | Temperature and heating rate | Holding time, h | Cooling mode |
Vacuum with a residual pressure not higher than 10-3 Torr. Art. or pure hydrogen with a dew point of not higher than minus 40 ° C. | (1125 ± 25) ° C not higher than 500 ° C / h | 3-6 | to 600 ° C at a rate not exceeding 200 ° C / h from 600 to 200 ° C at a rate of at least 400 ° C / h |
![]() |